LAE INTRODUCTION


LUBRICATED ALUMINUM ENTRY BOARD

ALUMINUM ENTRY BOARD
(Without Lubrication)
 
LAE FUNTIONALITY
LAE APPLICATION
LAE STRUCTURE

LAE TYPE

APERTURE

APPLICATION

ALTHK / COATING THK

LAE 0703

0.10 - 0.15mm

BGA 

70um/30um

LAE 1005

0.15 - 0.20mm

BGA

100um/50um

LAE 1505

0.20 - 0.30mm

High Density PCB

150um/50um

STORAGE METHOD

Improper technique and poor warehouse environment can damage LAE storage.

we suggest the LAE consumption within 2-3 hours after the bundle is unpack.


Temperature control at 20-40 Degree Celsius:  Lubrication layer is very sensitivity to heat.

Air conditioning and proper ventilation to control the heat index amid the hot months.


Moisture control at 60 +/-5%:  AL foil is moisture sensitive and easily oxidized .

A great solution is to use dehumidifiers to control moisture level especially at raining months.

 

COMPARISON ENTRY